We stock over 15 material grades of stainless and nickel round bar including: 304H, 310S, 317L, 321H, Alloy 347H, Alloy 20, Alloy C-276, Duplex 2205, Super Duplex 2507, 254SMO, Alloy 200, Alloy 400, Alloy 600, Alloy 625, Alloy 800H/HP, Alloy 825
304 stainless is a low-carbon (0.08% max) version of basic 18-8, also known as 302. Type 302 has 18% chromium and 8% nickel. Type 304 has a slightly lower strength than 302 due to its lower carbon content. Type 304 is used in welding applications, because the low carbon permits some exposure in the carbide precipitation range of 800° F - 1500° F without the need for post-annealing operations. However, the severity of the corrosive environments may necessitate annealing after welding or the use of 304L. Type 304L has a carbon content of 0.03% or less.
AVAILABILITY | |
---|---|
Seamless Pipe | 1/4" - 24" |
Weld Pipe | 1/2" - 36" |
Butt-Weld Fit | 1/2" - 36" |
Butt-Weld Fit SMLS | 1/2" - 36" |
Pressure Fittings | 1/4" - 4" |
150# Fittings/Nipples | 1/4" - 6" |
Valves | 1/2" - 24" |
Tubing | 1/4", 3/8", 1/2", 3/4", 1" |
Flanges | 1/2 |
TENSILE REQUIREMENTS | |
---|---|
TENSILE STRENGTH | (KSI) 70. |
YIELD STRENGTH | (KSI) 25. |
C | CR | MN | NI | P | S | SI | |||||
MAX | MAX | MAX | MAX | MAX | |||||||
0.035 | 18.0 - 20.0 | 2.0 | 8.0 - 13.0 | 0.045 | 0.030 | 1.00 | |||||
CHEMICAL COMPOSITION % |